Before using a new roll of DTF PET transfer film, take a few minutes to inspect it properly. Damage can occur during shipping, unpacking, handling, or installation, and some issues may only become visible during printing and transfer. This guide covers five essential checks, including safe ways to support and unwind the film, so you can identify potential problems before full production.
Section I. Inspect the Package Before Opening
Begin the inspection as soon as the film arrives. Shipping damage to the package may also affect the roll inside.
Check the outer package for:
- Crushed or dented corners, especially all eight corners of the box.
- Tears, punctures, openings, or visible scratches.
- Signs of moisture, water stains, or other shipping-related damage.
- Severe deformation or compression of the packaging.
If you notice obvious shipping damage, photograph the package before opening it and keep the original packaging for reference.
IMPORTANT: If the package is severely damaged or compressed, document its condition and contact Lancelot Technical Support before proceeding.
Section II. Remove the Film Roll and Check Its Overall Condition
Once the outer package appears acceptable, open the box carefully and remove the film roll without squeezing or bending it.
Proper handling:
- Use both hands to support the roll when lifting it out of the box.
- Keep the roll horizontal and evenly supported during removal.
- Avoid dropping, squeezing, bending, or placing excessive pressure on the roll.
- Place the roll on a clean, stable surface away from dust, sharp objects, and rough materials.
Before unwinding the film, inspect the roll itself. Use the table below as a quick reference.
| Inspection Area | What to Look For |
|---|---|
| Film roll | Visible scratches, impact marks, or deformation |
| Core | A crushed, bent, or deformed paper core |
| Roll edges | Uneven ends, damaged edges, or visible compression |
| Film layers | Areas where film layers appear stuck together |
| Coated surface | Dirt, stains, or visible surface contamination |
If you find an abnormality, take clear photos. Also record the film identification number printed inside the core and keep your order number available when contacting customer support.
Section III. Unwind the Film and Inspect the Surface
The outside of a roll may look normal even when defects are present farther inside. Unwind approximately 1 meter of film and inspect the exposed area under natural light or white lighting. The film should look flat and consistent, without obvious surface defects.
Choose one of the following handling methods to support the film during inspection:
Option 1 — Two-person inspection
- Have one person hold the unwound film horizontally and support it evenly, keeping the film stable and as flat as possible.
- Have the second person inspect the exposed surface for scratches, creases, stains, coating irregularities, or other visible defects.
Option 2 — One-person inspection
- Stand the film roll upright on a clean, stable tabletop.
- Gradually pull out the film while inspecting it. Keep the exposed section supported or lifted rather than laying it flat on the tabletop.
- Do not drag the film across the table or allow the coated surface to rub against it.
IMPORTANT: Do not lay the film horizontally on the tabletop and slide it during inspection. Friction against the table may cause scratches or other surface damage.
Check the exposed film for:
- Scratches and abrasions: visible lines, scuffs, or marks.
- Wrinkles and creases: folds, ripples, or uneven areas.
- Bubbles and pinholes: small openings or visible surface irregularities.
- Dust and particles: foreign substances, stains, or contamination.
- Coating irregularities: obvious streaks, spots, or uneven coating areas.
- Physical damage: tears, holes, or damaged edges.
If you find a localized defect, unwind a little more film to see whether it continues. If defects persist beyond approximately 3–4 meters, stop using the roll. Photograph or record the affected areas, note the film identification number and order number, and contact Lancelot Technical Support.
NOTE: Keep your hands clean and the inspection area free of dust and rough objects. Support the film throughout the inspection and minimize contact between the coated surface and other surfaces.
Section IV. Identify the Film Sides and Install the Roll Correctly
After completing the visual inspection, the next step is to identify the front and back sides of the PET film and install the roll according to your printer's requirements.
-
Check Both Sides of the Film Against the Light
Hold the PET film up to the light and examine the surface texture of both sides. For the Lancelot PET transfer film covered in this guide, the matte side is generally the printing side.
- Compare the surface appearance of both sides of the film.
- Identify the matte printing side and determine the correct film feeding direction according to your printer's requirements.
- If you cannot clearly identify the two sides, do not guess. Contact Lancelot Technical Support for confirmation before installation.
-
Install the Film Roll Correctly
Once you have identified the correct film side, install the roll according to your printer's loading instructions. After installation, check that the film is positioned correctly and lies flat. Make sure it feeds smoothly without visible wrinkles or misalignment.
Section V. Run a Small Test Print and Check the Results
A visual inspection cannot confirm every aspect of film performance. Before starting a full production job, print a small test design using your normal workflow.
Review the following stages:
Color Ink Reception
- Does the color image print evenly and completely?
- Are there unexpected ink smudges or spreading?
- Are there areas where the coating does not appear to receive the ink properly?
- Are the printed colors noticeably different from the design?
White Ink Performance
Check whether the white ink layer prints normally and aligns with the color image. Look for missing areas, uneven coverage, or other obvious abnormalities.
Powder Application
After printing with both color and white inks, allow the printed film to rest for approximately 3–5 minutes before applying TPU hot-melt adhesive powder. This gives the ink time to settle and helps reduce the chance of powder application affecting the printed image before the ink has stabilized. If both the color and white ink results look normal, proceed with powder application. Check that the TPU powder covers the printed areas evenly. Look for clumps, areas with insufficient powder, or excessive powder buildup in areas where it should not adhere.
Curing
Cure the printed film according to the requirements of the PET film, adhesive powder, and equipment. Make sure the powder melts evenly. Incorrect temperature or curing time may damage the transfer. Check for uneven melting or powder clumps.
Heat Pressing and Transfer
Place the cured transfer onto the garment and heat press according to the material requirements. Peel the PET film as instructed and check for complete transfer, missing details, uneven edges, or color issues.
Section VI. Conclusion & Technical Support
Inspecting a new PET film roll involves more than checking its outer packaging. Handle the roll carefully, inspect its overall condition, and support the exposed film while checking the surface. Use either a two-person horizontal support method or a one-person upright-roll method, and never drag the film across a tabletop.
Before full production, follow the printed direction arrow during installation and run a small test print. Evaluate color ink reception, white ink performance, powder application, curing, and the final transfer. If surface defects continue or test results are abnormal, stop using the roll and document the issue.
When contacting Lancelot Technical Support, provide the film identification number, order number, and clear photos or videos of the affected areas.
ADDITIONAL INFORMATION & SUPPORT RESOURCES
https://dtflancelot.com/products/lancelot-premium-dtf-transfer-roll-film-13-x328ft
Explore the Lancelot Premium DTF transfer film product details and specifications.
PET Film Installation Guidance
For help confirming the correct loading direction or installation method, contact Lancelot Technical Support for guidance applicable to your printer and film.
Have you ever discovered a PET film issue during unpacking or test printing? What did you notice? Share your experience in the comments.